各向异性增材制造构件的超声阵列全聚焦成像

徐娜 许路路 何方成

徐娜,许路路,何方成. 各向异性增材制造构件的超声阵列全聚焦成像[J]. 北京航空航天大学学报,2023,49(5):1063-1070 doi: 10.13700/j.bh.1001-5965.2021.0404
引用本文: 徐娜,许路路,何方成. 各向异性增材制造构件的超声阵列全聚焦成像[J]. 北京航空航天大学学报,2023,49(5):1063-1070 doi: 10.13700/j.bh.1001-5965.2021.0404
XU N,XU L L,HE F C. Total focusing imaging in anisotropic additive manufacturing components using ultrasonic array[J]. Journal of Beijing University of Aeronautics and Astronautics,2023,49(5):1063-1070 (in Chinese) doi: 10.13700/j.bh.1001-5965.2021.0404
Citation: XU N,XU L L,HE F C. Total focusing imaging in anisotropic additive manufacturing components using ultrasonic array[J]. Journal of Beijing University of Aeronautics and Astronautics,2023,49(5):1063-1070 (in Chinese) doi: 10.13700/j.bh.1001-5965.2021.0404

各向异性增材制造构件的超声阵列全聚焦成像

doi: 10.13700/j.bh.1001-5965.2021.0404
基金项目: 国家自然科学基金(51505449,52075049)
详细信息
    通讯作者:

    E-mail:bjxuna@163.com

  • 中图分类号: TB553

Total focusing imaging in anisotropic additive manufacturing components using ultrasonic array

Funds: National Natural Science Foundation of China (51505449,52075049)
More Information
  • 摘要:

    针对激光增材制造构件的各向异性特征,开展超声波传播特性研究,并基于群速度测量结果对常规超声阵列全聚焦成像算法进行优化。采用CIVA超声仿真软件对含有横通孔和平底孔缺陷的试样开展全聚焦仿真研究,结果表明,材料的各向异性对超声阵列全聚焦检测的成像质量、缺陷定位精度和缺陷分布范围均具有明显影响;开展全聚焦成像检测实验,结果表明,优化后的全聚焦成像算法能够实现激光增材制造钛合金试样中直径0.8 mm平底孔缺陷的准确检测,成像阵列性能指标(API)值减小至0.43,缺陷定位误差缩小至0.54 mm,检测能力和定位精度显著提高。

     

  • 图 1  激光增材制造金属材料中声速计算示意图

    Figure 1.  Schematic of wave velocity calculation in laser additive manufacturing materials

    图 2  激光增材制造金属材料中准纵波声速变化曲线

    Figure 2.  Velocity curves of quasi-longitudinal wave in laser additive manufacturing materials

    图 3  全聚焦成像算法原理图

    Figure 3.  Schematic of total focus imaging algorithm

    图 4  横通孔缺陷CIVA仿真模型

    Figure 4.  CIVA simulation model of horizontal through holes

    图 5  横通孔缺陷的常规全聚焦成像算法结果

    Figure 5.  Imaging results of horizontal through holes using conventional total focusing algorithm

    图 6  横通孔缺陷优化后的全聚焦成像算法结果

    Figure 6.  Imaging results of horizontal through holes using optimized total focusing algorithm

    图 7  横通孔缺陷优化前后的定位误差

    Figure 7.  Positioning error before and after optimization for horizontal through holes

    图 8  横通孔缺陷优化前后的成像API值

    Figure 8.  API value before and after optimization for horizontal through holes

    图 9  平底孔的CIVA仿真模型

    Figure 9.  CIVA simulation model of flat-bottom hole

    图 10  平底孔位置的局部图

    Figure 10.  Partial image of the flat-bottomed hole

    图 11  根据实验全矩阵数据拟合的声速曲线

    Figure 11.  Fitted velocity curves based on experimental FMC data

    图 12  X-Y面常规全聚焦成像算法的实验结果

    Figure 12.  Experimental results of X-Y surface using conventional total focusing imaging algorithm

    图 13  X-Y面优化的全聚焦成像算法的实验结果

    Figure 13.  Experimental results of X-Y surface using optimized total focusing imaging algorithm

    表  1  平底孔缺陷优化前后成像结果

    Table  1.   Imaging results before and after optimization for flat-bottom holes

    算法定位误差值/mmAPI值
    常规全聚焦成像0.8 1.63
    优化后的全聚焦成像0.141.66
    下载: 导出CSV
  • [1] 王华明, 张述泉, 汤海波, 等. 大型钛合金结构激光快速成形技术研究进展[J]. 航空精密制造技术, 2008, 44(6): 28-30. doi: 10.3969/j.issn.1003-5451.2008.06.023

    WANG H M, ZHANG S Q, TANG H B, et al. Research progress of laser rapid prototyping technology for large titanium alloy structure[J]. Aviation Precision Manufacturing Technology, 2008, 44(6): 28-30(in Chinese). doi: 10.3969/j.issn.1003-5451.2008.06.023
    [2] 王华明, 张述泉, 王向明. 大型钛合金结构件激光直接制造的进展与挑战(邀请论文)[J]. 中国激光, 2009, 36(12): 3204-3209. doi: 10.3788/CJL20093612.3204

    WANG H M, ZHANG S Q, WANG X M. Progress and challenges of laser direct manufacturing of large titanium structural components(invited paper)[J]. Chinese Journal of Lasers, 2009, 36(12): 3204-3209(in Chinese). doi: 10.3788/CJL20093612.3204
    [3] 王华明. 航空高性能金属结构件激光快速成形研究进展[J]. 航空制造技术, 2005, 48(12): 26-28. doi: 10.3969/j.issn.1671-833X.2005.12.024

    WANG H M. Research progress of laser rapid prototyping of aviation high performance metal structures[J]. Aeronautical Manufacturing Technology, 2005, 48(12): 26-28(in Chinese). doi: 10.3969/j.issn.1671-833X.2005.12.024
    [4] 张凤英, 陈静, 谭华, 等. 钛合金激光快速成形过程中缺陷形成机理研究[J]. 稀有金属材料与工程, 2007, 36(2): 211-215. doi: 10.3321/j.issn:1002-185x.2007.02.006

    ZHANG F Y, CHEN J, TAN H, et al. Research on forming mechanism of defects in laser rapid formed titanium alloy[J]. Rare Metal Materials and Engineering, 2007, 36(2): 211-215(in Chinese). doi: 10.3321/j.issn:1002-185x.2007.02.006
    [5] 阮雪茜, 林鑫, 黄春平, 等. TC4合金激光立体成形孔洞类缺陷的超声检测[J]. 中国激光, 2015, 42(12): 72-79.

    RUAN X Q, LIN X, HUANG C P, et al. Ultrasonic nondestructive testing of hole type defects in laser solid forming TC4 alloy[J]. Chinese Journal of Lasers, 2015, 42(12): 72-79(in Chinese).
    [6] ROMETSCH P A, PELLICCIA D, TOMUS D. Evaluation of polychromatic X-ray radiography defect detection limits in a sample fabricated from Hastelloy X by selective laser melting[J]. NDT & E International, 2014, 62: 184-192.
    [7] SONG Y F, ZI X H, FU Y D, et al. Nondestructive testing of additively manufactured material based on ultrasonic scattering measurement[J]. Measurement, 2018, 118: 105-112. doi: 10.1016/j.measurement.2018.01.020
    [8] ZIOLKOWSKI G, CHLEBUS E, SZYMCZYK P, et al. Application of X-ray CT method for discontinuity and porosity detection in 316L stainless steel parts produced with SLM technology[J]. Archives of Civil and Mechanical Engineering, 2014, 14(4): 608-614. doi: 10.1016/j.acme.2014.02.003
    [9] 杨平华, 史丽军, 梁菁, 等. TC18钛合金增材制造材料超声检测特征的试验研究[J]. 航空制造技术, 2017, 60(5): 38-42. doi: 10.16080/j.issn1671-833x.2017.05.038

    YANG P H, SHI L J, LIANG J, et al. Experimental research on ultrasonic characteristics of TC18 additive manufacturing titanium alloy[J]. Aeronautical Manufacturing Technology, 2017, 60(5): 38-42(in Chinese). doi: 10.16080/j.issn1671-833x.2017.05.038
    [10] 罗斯 J L. 固体中的超声波[M]. 何存富, 吴斌, 王秀彦, 译. 北京: 科学出版社, 2004: 21-23.

    ROSE J L. Ultrasonic waves in solid media[M]. HE C F, WU B, WANG X Y, translated. Beijing: Science Press, 2004: 21-23(in Chinese).
    [11] HOLMES C, DRINKWATER B, WILCOX P. The post-processing of ultrasonic array data using the total focusing method[J]. Insight-Non-Destructive Testing and Condition Monitoring, 2004, 46(11): 677-680. doi: 10.1784/insi.46.11.677.52285
    [12] DRINKWATER B W, WILCOX P D. Ultrasonic arrays for non-destructive evaluation: A review[J]. NDT & E International, 2006, 39(7): 525-541.
    [13] HOLMES C, DRINKWATER B W, WILCOX P D. Post-processing of the full matrix of ultrasonic transmit-receive array data for non-destructive evaluation[J]. NDT & E International, 2005, 38(8): 701-711.
    [14] 杨敬, 吴斌, 焦敬品, 等. 各向异性焊缝缺陷超声阵列全聚焦成像方法[J]. 声学学报, 2019, 44(1): 125-135. doi: 10.15949/j.cnki.0371-0025.2019.01.014

    YANG J, WU B, JIAO J P, et al. Total focus imaging of defects in anisotropic welds using ultrasonic array[J]. Acta Acustica, 2019, 44(1): 125-135(in Chinese). doi: 10.15949/j.cnki.0371-0025.2019.01.014
    [15] LI C, PAIN D, WILCOX P D, et al. Imaging composite material using ultrasonic arrays[J]. AIP Conference Proceedings, 2012, 1430(1): 897-904.
    [16] XU N, LI Y, ZHOU Z G. Ultrasonic nondestructive evaluation of composite components using advanced total focusing method[J]. Advanced Materials Research, 2013, 652-654: 1353-1356. doi: 10.4028/www.scientific.net/AMR.652-654.1353
    [17] ZHOU H P, HAN Z D, DU D, et al. A combined marching and minimizing ray-tracing algorithm developed for ultrasonic array imaging of austenitic welds[J]. NDT & E International, 2018, 95: 45-56.
  • 加载中
图(13) / 表(1)
计量
  • 文章访问数:  164
  • HTML全文浏览量:  44
  • PDF下载量:  22
  • 被引次数: 0
出版历程
  • 收稿日期:  2021-07-19
  • 录用日期:  2021-10-11
  • 网络出版日期:  2021-11-30
  • 整期出版日期:  2023-05-31

目录

    /

    返回文章
    返回
    常见问答