Citation: | Hou Bo, He Yuting, Cui Ronghong, et al. Fatigue crack monitoring of metallic structure based on coating sensor[J]. Journal of Beijing University of Aeronautics and Astronautics, 2013, 39(10): 1298-1302. (in Chinese) |
[1] Chang J C I.Aging aircraft science and technology issues and challenge and USAF aging aircraft program[J].Structural Integrity of Aging Aircraft,1995,47:1-7 [2] Wolfgang Ecke,Stephan Grimm.Optical fiber grating Sensor network basing on high-reliable fibers and components for space-craft health monitoring .SPIE,2001,4328:160-167 [3] Schubert F.Basic principles of acoustic emission tomography[J].Journal of Acoustic Emission,2004,22:147-158 [4] Fukunaga H,Hu N,Chang F K.Structural damage identification using piezoelectric sensors[J].International Journal of Solids and Structures,2002,39(2):393-418 [5] Wheatley G,Clellan K L M.Remote periodic monitoring of fatigue crack prone areas by CVMTM—the H-53 experience[C]//6th Joint FAA/DoD/NASA Aircraft Conference on Aging Aircraft.Missouri:FAA,2002 [6] 杜金强,何宇廷,崔荣洪,等.基于电位法原理的金属结构裂纹监测传感器研究[J].南京航空航天学报,2010,42(3):387-391 Du Jinqiang,He Yuting,Cui Ronghong,et al.Research on surface crack monitoring sensor of metallic structure based on electric potential method[J].Journal of Nanjing University of Aeronautics and Astronautics,2010,42(3):387-391(in Chinese) [7] Todoroki A, Tanaka Y.Delamination identification of crossply graphite/epoxy composite beams using electric resistance change method[J].Compos Sci Technol,2002,62(6):29-39 [8] Schueler R,Joshi S P,Schulte K.Damage detection in CFRP by electrical conductivity mapping[J]. Compos Sci Technol,2001,61(9):21-30 [9] 顾迅.现代表面技术的应用[J].金属热处理,1999(4):1-6 Gu Xun.Application of modern surface technology[J].Heat Treatment of Metals,1999(4):1-6(in Chinese) [10] 张胜宝,师玉英,张旭.铝合金硬质阳极氧化工艺研究[J].电镀与精饰,2011,33(8):43-46 Zhang Shengbao,Shi Yuying,Zhang Xu.Hard anodizing technology of aluminum alloy[J].Plating and Finishing,2011, 33(8) :43-46(in Chinese) [11] 韩克,欧忠文,蒲滕,等.铝及铝合金硬质阳极氧化的研究进展[J].表面技术,2011,40(5):92-96 Han Ke,Ou Zhongwen,Pu teng,et al.Development of hard anodizing of aluminum and aluminum alloy[J].Surface Technology,2011,40(5):92-96(in Chinese) [12] 刘高杰,邓春枝.HCD空心阴极离子镀工艺研究[J].中国钼业,1997(4):46-48 Liu Gaojie,Deng Chunzhi.The technology research of hollow cathode deposition[J].China Molybdenum Industry,1997(4):46-48 (in Chinese) [13] 王基茹,蔡健平,丁鹤雁,等.国内外非铬航空涂层的研究进展[J].现代涂料与涂装,2005(2):39-41 Wang Jiru,Cai Jianping,Ding Heyan,et al.Research progress of non-chromate coatings for aircraft in the world[J].Modern Paint and Finishing,2005(2):39-41(in Chinese)
|