Citation: | Xie Weijie, Li Di, Hu Yanling, et al. Half-Quantification of High Strength Aluminum Alloy's Corrosion Rank[J]. Journal of Beijing University of Aeronautics and Astronautics, 1999, 25(5): 502-504. (in Chinese) |
1. Sprowls D O, Sammerson T J, Loftin F E. Exfoliation corrosion testing of 7075 and 7178 Al alloys — laterin report on atmospheric exposure tests. In:ASTM STP 558. [s.l.]:American Society for Testing and Materials,1974.99~113 2. Lifka, B W, Sprowls D O. Relationship of accelerated test methods for exfoliation in 7XXX series aluminum alloys with exposure to a seacoast atmosphere, corrosion in natural environments.In:ASTM STP 558.[s.l.]:American Society for Testing and Materials, 1974.306~333 3. 谢伟杰. LY12CZ和7075T7351铝合金耐腐蚀寿命预测的探讨:[学位论文].北京:北京航空航天大学材料科学与工程系,1998 4. 韩於羹. 应用数理统计. 北京:北京航空航天大学出版社,1993
|